Photo 2 - Typed page 5" behind the anti-glare sheet
Photo 3 - Typed page immediately behind the anti-glare sheet (touching)
Polycarbonate sheet readily absorbs moisture from the air. Eventually the water content will reach 0.2% by weight.
", it’s finally time to share what we’ve learned about printing with Polycarbonate. As we recently announced, pre-orders for Polycarbonate in both 3mm and 1.75mm diameters are available. It took us awhile to get the details sorted out, but we’ set for a ship date of January 30, 2012. There’s a whole world of materials out there for that hungry printer on your desk, and we plan to dish up a feast.
Larger prints were prone to peeling off the print-bed if they contained too many long aligned traces; examining the datasheet revealed that this PC had a mold release additive, great for injection molding, not so great for us (the PC available for pre-order does NOT have this additive and should stick easier to print beds). Small objects printed fine with no warping but we needed to find a way to keep large prints held down; enter ABS Glue. Painting a thin coat of that on the bed before printing completely eliminated peeling and warping, we could even print without the heated bed and maybe see only the smallest of curling on the corners of large prints.
To test the effect that leaving the PC out in open air was having we split up the sample; one went in the dehydrator, another into one lucky fellow’s home for a couple days. Printing with them revealed obvious difference. The dried sample printing clear and smooth without hiccups, the sample that had gone through a few days of home living printed white and would occasionally pop and bubble. Comparing prints side by side shows an obvious reduction in clarity and surface quality for the undried filament. While we haven’t done any numerical testing of compared strength, the moisture laden sample felt more brittle and prints made from it break much easier. Objects printed with the dried PC are clear and strong. Returning to the T-Slot it is clear to see the differences between dry filament and filament left where humidity is not controlled. Click the pictures below for high resolution to really see the differences.
All in all, a very simple material to start printing with. As long as it is kept relatively free of moisture and/or dried, printed objects turn out looking good, are well bonded and very strong. This is a plastic that can take a bit more of a beating and stand a little more heat, not bad if you need something close to you’re hotend such as a cooling duct. Printing parameters we’re using so far are:
We’ve got it on pre-order, prices include shipping within the USA, world wide shipping is available through ourinternational ordering form with an additional $9.00 to match the increased shipping cost of the flat rate mailers we are able to use. We have a scheduled ship date of January 30, 2012 after which the product can batch with other orders and the shipping cost will be subtracted back out of the product listing if we have any remaining inventory. Go on over and grab some in either 3mm or 1.75mm."
A question that we are frequently asked is how thick is transparent armor made from glass and polycarbonate?
In the final blog post of this trilogy we will discuss Iridescence and how it can cause a rainbow effect on abrasion resistant coated Polycarbonate sheet. We will also discuss how the rainbow effect can be minimized.
In the last post we discussed how stresses in Polycarbonate can cause the material to become Anisotropic and exhibit Birefringent properties. Light waves parallel to the stress direction will travel through the sheet at a different speed than the light waves perpendicular to the stress direction.
One question that we are often asked about Polycarbonate is what causes the rainbow like patterns on coated sheet and how can they be eliminated.